Discuss your material challenge
Solutions / Fire performance

Fire behaviour is a property of the system, not of the additive.

Wood species, panel structure, treatment level, geometry, later coatings and the test standard all change the result. We therefore work on a defined build-up, test it, and tie every statement to that test.

What we have measured

Corner specimen of three-layer spruce after the Single Burning Item test, charred along the inner corner
Corner specimen after the SBI test

D-s1,d0 C-s1,d0

Preliminary Single Burning Item test to EN 13501-1. Three-layer spruce. TÜV SÜD, 03/2025. The class applies to this tested build-up only.

Total heat releaseEnergy given off during the test
15.3 MJ11.1 MJ
−27 %
Fire growth rate (FIGRA 0.2)How fast the fire builds up
480 W/s250 W/s
−48 %
Smoke growth rate (SMOGRA)How fast smoke density rises
1.31 m²/s²0
to zero
Total smoke productionWent up. The formulation is being adapted for this.
16.1 m²29.2 m²
+81 %

UntreatedTreated

The first test: a flame on thin fir.

Berner Fachhochschule, 02/2024. A flame was held to the lower edge of each specimen for 30 seconds.

  • Treated specimens thicker than 4 mm did not ignite. All untreated control specimens did.
  • Treated specimens under 3 mm burned only while the flame touched them, then went out by themselves.
  • The thicker treated specimens lost very little weight.

Fir, untreated

Untreated fir specimen, 4 mm, charred over most of its height
4 mm
Untreated fir specimen, 6 mm, charred over more than half its height
6 mm

Fir, impregnated with PURE B210

Treated fir specimen, 2 mm, narrow char mark
2 mm
Treated fir specimen, 3 mm, small char mark at the lower edge
3 mm
Treated fir specimen, 4 mm, small char mark at the lower edge
4 mm
Treated fir specimen, 5 mm, small char mark at the lower edge
5 mm

Where it applies

  • Solid wood and timber elements
  • Engineered wood products
  • Natural-fibre and biomass boards
  • Insulation and acoustic materials

What is still open

  • Smoke production rose in the SBI test. The formulation is being adapted.
  • The SBI result is preliminary and covers one build-up of three-layer spruce.
  • A classification for your product needs a test on your product.

The usual way in is a Validate programme on your own substrate.

Tell us the substrate, the problem and what success has to look like.

Discuss your material challenge