What has been tested, by whom, and what came out.

A test result belongs to one substrate, one build-up, one method and one jurisdiction. We keep it that way and do not turn a single result into a claim for the whole portfolio.

Product facts

What a product is and contains, as written in its technical and safety data sheets.

Test facts

What a lab or a field site measured, valid for the tested substrate, system and method.

Development directions

What we are working towards. These are aims and carry a status label, never a performance figure.

Single Burning Item test, three-layer spruce

Corner specimen of three-layer spruce after the Single Burning Item test, charred along the inner corner
Corner specimen after the SBI test

D-s1,d0 C-s1,d0

Preliminary Single Burning Item test to EN 13501-1. Three-layer spruce. TÜV SÜD, 03/2025. The class applies to this tested build-up only.

Total heat releaseEnergy given off during the test
15.3 MJ11.1 MJ
−27 %
Fire growth rate (FIGRA 0.2)How fast the fire builds up
480 W/s250 W/s
−48 %
Smoke growth rate (SMOGRA)How fast smoke density rises
1.31 m²/s²0
to zero
Total smoke productionWent up. The formulation is being adapted for this.
16.1 m²29.2 m²
+81 %

UntreatedTreated

Flame test on fir

Berner Fachhochschule, 02/2024. Flame on the lower edge for 30 seconds.

  • Treated specimens thicker than 4 mm did not ignite. All untreated controls did.
  • Treated specimens under 3 mm self-extinguished once the flame was removed.
  • Untreated specimens had to be put out by hand.

Fir, untreated

Untreated fir specimen, 4 mm, charred over most of its height
4 mm
Untreated fir specimen, 6 mm, charred over more than half its height
6 mm

Fir, impregnated with PURE B210

Treated fir specimen, 2 mm, narrow char mark
2 mm
Treated fir specimen, 3 mm, small char mark at the lower edge
3 mm
Treated fir specimen, 4 mm, small char mark at the lower edge
4 mm
Treated fir specimen, 5 mm, small char mark at the lower edge
5 mm

All seven tests

  1. Flame test on firBerner Fachhochschule
    02/2024

    Treated specimens over 4 mm did not ignite. Thinner ones self-extinguished.

    Completed
  2. Preliminary SBI on three-layer spruceTÜV SÜD
    03/2025

    Heat release and fire growth down, smoke volume up. See the figures above.

    Completed, preliminary
  3. Weathering of Swiss larchAecherli Holz AG
    since 08/2025

    Untreated boards turn black. Treated boards darken at first, then lighten, and splash stains do not show.

    Ongoing
  4. Weathering of robiniaPrivate garden fence
    08/2023 to 09/2025

    After two years: no noticeable cracks or splinters on treated slats. Untreated slats blackened, partly from fungi.

    Two years observed
  5. Water-resistant coatings with grapheneRIC-2D, Khalifa University
    07/2025

    The liquid graphene formulation showed promise for water repellency and corrosion protection. Results are semi-quantitative.

    Completed, to be confirmed
  6. Public benches in larchBURRI public elements AG
    since 08/2025

    Greying, ageing and the lifespan of the paint coat on treated bench slats.

    Ongoing
  7. Binder for hemp and straw panelsIn-house
    since 08/2025

    Panels of hemp shives and of straw formed successfully. Mechanical tests, water stability and swelling are pending.

    Tests pending

Test reports, technical data sheets and safety data sheets are available on request. Request documents